What grade of wet and dry paper or what colour scratch pad is used to give a prepreg part a key ready for clearcoat ?.

Cheers!
Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
400 can work, it's what I spray base coats on but I find it a bit rough for clear coat, you can often still see the scratches. This will depend on your coating though, thinner ones will fill less obviously. 