What grade of wet and dry paper or what colour scratch pad is used to give a prepreg part a key ready for clearcoat ?.
Cheers!
|
By Hanaldo - 9/11/2015 4:17:13 PM
400 can work, it's what I spray base coats on but I find it a bit rough for clear coat, you can often still see the scratches. This will depend on your coating though, thinner ones will fill less obviously.
|
|