What grade of wet and dry paper or what colour scratch pad is used to give a prepreg part a key ready for clearcoat ?.

Cheers!
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Depends on the coating system. I use Duratec Sunshield, which is a high build coating and fills scratches really well, so for that you would use 120-180 grit. 

For regular coatings though, that is EXTREMELY course. So if you are using a regular automotive paint, then you'd want to be scuffing it up with 600-800 grit. I've seen people use as high as 1200 grit, but I would be questioning how good the mechanical adhesion is with that level of key. 
MarkMK
MarkMK
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 338, Visits: 2K
A bit off-topic from Bob's question, but does anyone know how to get hold of Duratec Sunshield in the UK?

Sounds like a useful product for those without access to automotive spray facilities but struggling to find it here
Rich (Staff)
Rich (Staff)
Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)
Group: Administrators
Posts: 167, Visits: 4.6K
I find 400 grit is ideal for surface prep, obviously ensuring that the surface is cleaned and free from any water or grease before clear coating.
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
400 can work, it's what I spray base coats on but I find it a bit rough for clear coat, you can often still see the scratches. This will depend on your coating though, thinner ones will fill less obviously. 