Hi there,
New to the forum so good day to everyone.

I want to eventually convert all my plastics (fairings) to CF and having to wet lay as I will go to vacuum bagging at some point in the future.

I want to start with simple molds first but a few have flanges/ mounting points behind the plastics. What's the best way to do this? Been watching vids on here and pootube.

If I can upload an image will do so asap.

Until then many thanks.
Jay
Reply
VVS
VVS
Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)
Group: Moderators
Posts: 226, Visits: 334
Hi jay,

give it a go. You need to make the panel in cf then glue any tabs on the rear using anything you can to fit.

I'm doing a similar thing to you and am a little further down the road so should be able to answer a few of your questions.

Ive found the green epoxy tooling gel fairly easy to use as it doesn't smell like the uni mould, that said the uni can be left between each stage so this can be useful if time is tight.

I'd advise putting edges on the moulds as you will want to infuse once you start, its kind of addictive.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
simyboye - 10 Years Ago
redeye - 10 Years Ago
simyboye - 10 Years Ago
redeye - 10 Years Ago
VVS - 10 Years Ago
simyboye - 10 Years Ago
redeye - 10 Years Ago
simyboye - 10 Years Ago
redeye - 10 Years Ago
simyboye - 10 Years Ago
djtd - 10 Years Ago
Jacopo Carbonio - 10 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search