Resin Infusion
»
Spiral Wrap Diameter
Spiral Wrap Diameter
Post Reply
Like
3
Spiral Wrap Diameter
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
CFdavid
CFdavid
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 3,
Visits: 5
which diameter works best for vacuum infusion process? both resin feed side and vacuum side.
Reply
Like
3
Reply
Matthieu Libeert
Matthieu Libeert
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
I always use spiral tube all around my part, on the flange... to achieve a better vacuum for the entire part. The spiraltube is connected to the vacuumpump...
I set the injectionpoint in the middle of the part without spiral
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Spiral Wrap Diameter
CFdavid
-
13 Years Ago
The infusion spiral i use is 5mm ID. always been fine for what ive needed. You only need to use...
Warren
-
13 Years Ago
thank you
CFdavid
-
13 Years Ago
thank you
CFdavid
-
13 Years Ago
I always use spiral tube all around my part, on the flange... to achieve a better vacuum for the...
matthieutje65
-
13 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search