which diameter works best for vacuum infusion process? both resin feed side and vacuum side.
By matthieutje65
-
5/13/2012 5:39:46 PM
I always use spiral tube all around my part, on the flange... to achieve a better vacuum for the entire part. The spiraltube is connected to the vacuumpump...
I set the injectionpoint in the middle of the part without spiral