I always use spiral tube all around my part, on the flange... to achieve a better vacuum for the entire part. The spiraltube is connected to the vacuumpump...
I set the injectionpoint in the middle of the part without spiral Smile

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




CFdavid
CFdavid
Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)
Group: Forum Members
Posts: 3, Visits: 5
thank you
CFdavid
CFdavid
Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)
Group: Forum Members
Posts: 3, Visits: 5
thank you
Warren
Warren
Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)
Group: Administrators
Posts: 214, Visits: 782
The infusion spiral i use is 5mm ID. always been fine for what ive needed.

You only need to use spiral on the resin feed side of the infusion.
CFdavid
CFdavid
Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)
Group: Forum Members
Posts: 3, Visits: 5
which diameter works best for vacuum infusion process?  both resin feed side and vacuum side.  