Hello guys , Had my 1st try with MTI hose today , couldn't get the bag to vac down . Pulled everything apart and connected the MTI hose directly to the vac hose and pulled 100% vac ??   What am I doing wrong ? MTI hose didn't seem to let air through ??    Tried the traditional way with spiral and resin break and infusion seemed to go well . I will pop it tomorrow to see what the surface looks like . 
Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
MTI definitely flows less air, it often takes my 5cfm pump a good 5 minutes to pull down a small 30x30cm bag whereas without it that same size bag would be pulled down almost straight away. 