Hello guys , Had my 1st try with MTI hose today , couldn't get the bag to vac down . Pulled everything apart and connected the MTI hose directly to the vac hose and pulled 100% vac ??   What am I doing wrong ? MTI hose didn't seem to let air through ??    Tried the traditional way with spiral and resin break and infusion seemed to go well . I will pop it tomorrow to see what the surface looks like . 
Reply
whitecel
whitecel
Supreme Being (133 reputation)Supreme Being (133 reputation)Supreme Being (133 reputation)Supreme Being (133 reputation)Supreme Being (133 reputation)Supreme Being (133 reputation)Supreme Being (133 reputation)Supreme Being (133 reputation)Supreme Being (133 reputation)
Group: Forum Members
Posts: 19, Visits: 39
Are you sure you set it up correctly?  Sealed one end with gum tape?  Sure you had a good seal on the bag?  I noticed with the MTI hose, it takes a few seconds longer for the vacuum to be pulled through.