Hi all, going to be infusing a three part mould that's around 3/4 mtr square,

what kind of silicon are you guys using and where do you apply the silicon,

just around the edges, all over the joint flanges etc.




Chris.
Reply
VVS
VVS
Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)
Group: Moderators
Posts: 226, Visits: 334
Thanks matt for the tape attack.

I will try silicon first and have some red heat proof 100% silicon that will show up well against the black gel coat, hopefully non of the red pigment will cross to the part, only one way to find out.