By VVS - 4/2/2015 8:45:14 PM

Hi all, going to be infusing a three part mould that's around 3/4 mtr square,

what kind of silicon are you guys using and where do you apply the silicon,

just around the edges, all over the joint flanges etc.




Chris.
By VVS - 4/3/2015 5:04:30 PM

Thanks matt for the tape attack.

I will try silicon first and have some red heat proof 100% silicon that will show up well against the black gel coat, hopefully non of the red pigment will cross to the part, only one way to find out.