Ha! Thank you.

The insulation is rock wool 30mm slab, I had to buy a pack of 12 sheets (1200x600mm) so the remainder is going in my loft. 

Perforated sheet steel with the edges folded over 25mm all round the edge forms the baffle / base over the elements.
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Genius! 

What did you use for insulation?? And the grated floor? 
Bonobo
Bonobo
Supreme Being (711 reputation)Supreme Being (711 reputation)Supreme Being (711 reputation)Supreme Being (711 reputation)Supreme Being (711 reputation)Supreme Being (711 reputation)Supreme Being (711 reputation)Supreme Being (711 reputation)Supreme Being (711 reputation)
Group: Forum Members
Posts: 85, Visits: 1.2K
the cabinet was the most expensive item at £70
internal dimensions with the insulation in place is approx 110cm x 35cm x 40cm
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
clever thinking with the IKEA cabinet! Wink

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




Bonobo
Bonobo
Supreme Being (711 reputation)Supreme Being (711 reputation)Supreme Being (711 reputation)Supreme Being (711 reputation)Supreme Being (711 reputation)Supreme Being (711 reputation)Supreme Being (711 reputation)Supreme Being (711 reputation)Supreme Being (711 reputation)
Group: Forum Members
Posts: 85, Visits: 1.2K
BINGO! Ikea cabinet
elements are from an oven spares supplier 2 x 1000w
Dravis
Dravis
Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
That looks like an IKEA steel cabinet  .. Hehe   Where did you get the heater elements from?

Nice work ... good thinking ...

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
davro
davro
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 300, Visits: 2.2K
Nice work!

I have been thinking about upgrading my ghetto composite table/oven recently and this has given me some ideas Wink



David Stevens
YouTubeComment | Rate | Subscribe
Instagram

Composite Projects
Body Package for Dax Rush
RC Car Touring Body 1/10 Scale


Bonobo
Bonobo
Supreme Being (711 reputation)Supreme Being (711 reputation)Supreme Being (711 reputation)Supreme Being (711 reputation)Supreme Being (711 reputation)Supreme Being (711 reputation)Supreme Being (711 reputation)Supreme Being (711 reputation)Supreme Being (711 reputation)
Group: Forum Members
Posts: 85, Visits: 1.2K


http://www.talkcomposites.com/Uploads/Images/cd701533-e912-45a2-ae34-51aa.JPGhttp://www.talkcomposites.com/Uploads/Images/2dcf1958-5ea9-415c-be39-ae91.JPGhttp://www.talkcomposites.com/Uploads/Images/ee1bf0da-fc9b-4980-9007-0793.JPGhttp://www.talkcomposites.com/Uploads/Images/1842fde0-73d0-4bd5-aa84-1b8c.JPGhttp://www.talkcomposites.com/Uploads/Images/95003f9d-f3ec-4c42-a600-0be3.JPGhttp://www.talkcomposites.com/Uploads/Images/958580b4-8b36-4718-80e1-173c.JPG

Built using all new, off the shelf parts