Bonobo
Bonobo
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 85,
Visits: 1.2K
Built using all new, off the shelf parts
Reply
Like
3
davro
davro
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 300,
Visits: 2.2K
Nice work!
I have been thinking about upgrading my ghetto composite table/oven recently and this has given me some ideas
David Stevens
YouTube
: 
Comment | Rate | Subscribe
Instagram
Composite Projects
Body Package for Dax Rush
RC Car Touring Body 1/10 Scale
Reply
Like
2
Dravis
Dravis
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 592,
Visits: 1.9K
That looks like an IKEA steel cabinet ..
Where did you get the heater elements from?
Nice work ... good thinking ...
"Sapere Aude"... Dare to KNOW!
The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...
103% of all people do not understand statistics...
Do not adjust our mind, theres a fault in reality :-)
Reply
Like
3
Bonobo
Bonobo
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 85,
Visits: 1.2K
BINGO! Ikea cabinet
elements are from an oven spares supplier 2 x 1000w
Reply
Like
3
Matthieu Libeert
Matthieu Libeert
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
clever thinking with the IKEA cabinet!
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
3
Bonobo
Bonobo
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 85,
Visits: 1.2K
the cabinet was the most expensive item at £70
internal dimensions with the insulation in place is approx 110cm x 35cm x 40cm
Reply
Like
3
Hanaldo
Hanaldo
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Genius!
What did you use for insulation?? And the grated floor?
Reply
Like
2
Bonobo
Bonobo
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 85,
Visits: 1.2K
Ha! Thank you.
The insulation is rock wool 30mm slab, I had to buy a pack of 12 sheets (1200x600mm) so the remainder is going in my loft.
Perforated sheet steel with the edges folded over 25mm all round the edge forms the baffle / base over the elements.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search