My completed curing oven build

http://www.talkcomposites.com/Topic15717.aspx

By Bonobo - 3/20/2015 9:58:07 AM



http://www.talkcomposites.com/Uploads/Images/cd701533-e912-45a2-ae34-51aa.JPGhttp://www.talkcomposites.com/Uploads/Images/2dcf1958-5ea9-415c-be39-ae91.JPGhttp://www.talkcomposites.com/Uploads/Images/ee1bf0da-fc9b-4980-9007-0793.JPGhttp://www.talkcomposites.com/Uploads/Images/1842fde0-73d0-4bd5-aa84-1b8c.JPGhttp://www.talkcomposites.com/Uploads/Images/95003f9d-f3ec-4c42-a600-0be3.JPGhttp://www.talkcomposites.com/Uploads/Images/958580b4-8b36-4718-80e1-173c.JPG

Built using all new, off the shelf parts
By Bonobo - 3/20/2015 6:11:12 PM

Ha! Thank you.

The insulation is rock wool 30mm slab, I had to buy a pack of 12 sheets (1200x600mm) so the remainder is going in my loft. 

Perforated sheet steel with the edges folded over 25mm all round the edge forms the baffle / base over the elements.