Hi,

What is the best way to cut / trim and finish the edges of Kevlar / aramid parts after demolding so that they do not end up with a 'furry' edge?

I am using a high speed Dremel-type tool with a diamond cutting disc (the carbide discs are too thin and delicate, and shatter too easily) to cut the cured Kevlar but it leaves a slightly fuzzy edge. Is there a way to finish these edges so that they have a cleaner finish (like sanded carbon edges)?

Thanks,

Phil.
                                                    
Reply
philiplardner
philiplardner
Supreme Being (360 reputation)Supreme Being (360 reputation)Supreme Being (360 reputation)Supreme Being (360 reputation)Supreme Being (360 reputation)Supreme Being (360 reputation)Supreme Being (360 reputation)Supreme Being (360 reputation)Supreme Being (360 reputation)
Group: Awaiting Activation
Posts: 25, Visits: 65
Thanks guys - I'll give those methods a try.

Much appreciated,

Phil.
carbon-dragon.ihpa.ie
Edited 10 Years Ago by philiplardner
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search