Crixus
Crixus
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Awaiting Activation
Posts: 1,
Visits: 14
So I am using AeroMarine Epoxy Resin #300 and Hardener #21 along with MG Chemicals Epoxy Mold Release. I mixed the epoxies together and placed my first coat on the silicone mold and let it stand for a couple hours. Then I placed the carbon fiber sheets down and coated each layer with more epoxy. When I take it out, I'm getting a white film on the surface that is touching the silicone mold. I've tried searching for the solution with no luck. So I am hoping you all can help me. Thanks you. For those curious, this is a UFO body for a quad copter.
Reply
Like
2
Reply
Fasta
Fasta
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 468,
Visits: 3.5K
When I have seen white ish resin it is usually moisture that has gotten into the curing resin. I think!
Otherwise it may be some issue with the silicone reacting to the resin?? Just a guess.
Fastacraft Facebook page
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Getting a whitish film on my carbon fiber
Crixus
-
11 Years Ago
from what i understand you got air pockets where no resin on carbon and problem with release agent.
TomDesign
-
11 Years Ago
When I have seen white ish resin it is usually moisture that has gotten into the curing resin. I...
Fasta
-
11 Years Ago
it looks as though you arent getting decent consolidation into the features of the part,areyou...
scottracing
-
11 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search