Group: Forum Members
Posts: 460,
Visits: 5.2K
|
it looks as though you arent getting decent consolidation into the features of the part,areyou vacuum bagging it at all? I would suggest cutting stars over the round features on the first ply then putting a cap over the top, and if you can trying to put it into a vacuum bag, even the clothes type ones using a suitable plastic film as a barrier soit doesnt stick to the bag.
|