Getting a whitish film on my carbon fiber


Author
Message
scottracing
scottracing
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
it looks as though you arent getting decent consolidation into the features of the part,areyou vacuum bagging it at all? I would suggest cutting stars over the round features on the first ply then putting a cap over the top, and if you can trying to put it into a vacuum bag, even the clothes type ones using a suitable plastic film as a barrier soit doesnt stick to the bag.
Fasta
Fasta
Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
When I have seen white ish resin it is usually moisture that has gotten into the curing resin. I think!

Otherwise it may be some issue with the silicone reacting to the resin?? Just a guess.




TomDesign
TomDesign
Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)
Group: Forum Members
Posts: 454, Visits: 2.5K
from what i understand you got air pockets where no resin on carbon and problem with release agent.
Crixus
Crixus
Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)
Group: Awaiting Activation
Posts: 1, Visits: 14
So I am using AeroMarine Epoxy Resin #300 and Hardener #21 along with MG Chemicals Epoxy Mold Release. I mixed the epoxies together and placed my first coat on the silicone mold and let it stand for a couple hours. Then I placed the carbon fiber sheets down and coated each layer with more epoxy. When I take it out, I'm getting a white film on the surface that is touching the silicone mold. I've tried searching for the solution with no luck. So I am hoping you all can help me. Thanks you. For those curious, this is a UFO body for a quad copter.
http://www.talkcomposites.com/Uploads/Images/905774c1-8489-4d53-9ae2-578e.jpghttp://www.talkcomposites.com/Uploads/Images/8d59ba08-bdaa-4d7a-b808-954e.jpghttp://www.talkcomposites.com/Uploads/Images/f28394c8-4c00-445c-aa97-c16e.jpg