When infusion goes bad!


Author
Message
FLD
FLD
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
After many years vac-bagging and avoiding infusion I was tempted to try it after some gentle persuasion.  Freakin' awesome!  Not hard and great results.  Yay!

However, I recently made a booboo.  Infusing a 1.2m x 0.2m part; 4x200g with 6x200g in places; peel ply, mesh, bag.  I opened the inlet clamp and it seemed to stick.  A little jiggle and the resin shot through, not all the way but a good chunk was done in about 20 sec.  Bugger!  Let it flow at a more sensible rate to finish up.  I let a little more flow in on completion but as expected its pinhole-tastic on the fast bit.  Is there any contingency for things like this, ie should I have let more resin flow through or is it a once the damage is done thats it?

If there's a fix it would be good to have a list of problems and solutions.
Reply
FLD
FLD
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
Thanks guys Smile  Some great tips.  I am indeed using the wingnut clamps and will give these ideas a try out on the next panel. 