Group: Forum Members
Posts: 468,
Visits: 2.7K
|
After many years vac-bagging and avoiding infusion I was tempted to try it after some gentle persuasion. Freakin' awesome! Not hard and great results. Yay!
However, I recently made a booboo. Infusing a 1.2m x 0.2m part; 4x200g with 6x200g in places; peel ply, mesh, bag. I opened the inlet clamp and it seemed to stick. A little jiggle and the resin shot through, not all the way but a good chunk was done in about 20 sec. Bugger! Let it flow at a more sensible rate to finish up. I let a little more flow in on completion but as expected its pinhole-tastic on the fast bit. Is there any contingency for things like this, ie should I have let more resin flow through or is it a once the damage is done thats it?
If there's a fix it would be good to have a list of problems and solutions.
|