What resin would be best suited to coat toughened glass?


Author
Message
cheekygr1n
cheekygr1n
Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)
Group: Forum Members
Posts: 2, Visits: 7
I am thinking of constructing a shower enclosure using toughened glass sheets (up to 1400mm x2500mm x8mm thick), and coating the back of the glass with a coloured gel coat / resin  / epoxy.

I have been quoted £2600 to purchase factory made coloured glass splash backs which is outside of my budget!

A plain / metallic grey (aluminium powdered?) would be the preferred finished colour.

UV stability will not be much of an issue due to very low natural light levels indoors.

I would like some advise on what would be the most suited gel coat / resin / epoxy that would bond well to glass, and could provide a good uniform colour (not opaque).

Thanks, Sean.
Reply
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Hi Sean, not sure if you are wanting to make the actual enclosure or the wall panels as you mention splash backs?
If its the wall panels there is a post I did under Projects - Other - Composites Around The Home. Sorry cant seem to add a link on my phone.
Warren

Carbon Copies Ltd
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search