What resin would be best suited to coat toughened glass?

http://www.talkcomposites.com/Topic13535.aspx

By cheekygr1n - 11/1/2014 4:57:02 PM

I am thinking of constructing a shower enclosure using toughened glass sheets (up to 1400mm x2500mm x8mm thick), and coating the back of the glass with a coloured gel coat / resin  / epoxy.

I have been quoted £2600 to purchase factory made coloured glass splash backs which is outside of my budget!

A plain / metallic grey (aluminium powdered?) would be the preferred finished colour.

UV stability will not be much of an issue due to very low natural light levels indoors.

I would like some advise on what would be the most suited gel coat / resin / epoxy that would bond well to glass, and could provide a good uniform colour (not opaque).

Thanks, Sean.
By Dravis - 11/6/2014 4:56:38 PM

If you're buying the glass panels, then order them matted on one side... job done..

The acids for etching glass are truly nasty stuff ... you do not want to play around with that..     (flourine acid ... yiikes...  Sick)

If the paint is done properly, then bonding with normal building bonding adhesives will not damage it, you may need to wet sand the paint very lightly to get the stuff to bond properly.