Is it just to add a "coloured background"/ prevent "see-through" of the glass? If that's the case, you can simply sand-blast the back side of the glass, and use 2-component auto spray paint on the matted surface, it will be just as strong as a layer of epoxy or poly resin.  And you can get it any colour you like 

The Audi "Dolphin Grey Metallic" is very nice ......
I did a dark edge around my bathroom mirror that way, taped up the area not to loose its silver reflective backing, sandblasted it ,taped up the outer edge leaving a 4 cm wide matte glass area for the LED backlight, and a  matte dark grey edge.                   
			            
				
			            "Sapere Aude"... Dare to KNOW!
The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...
103% of all people do not understand statistics...
Do not adjust our mind, theres a fault in reality :-)