Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi All,

As some of you may have noticed, we added a new very special offer to our website last Friday which was our new 'Black Stuff' carbon fibre cloth. There's plenty of information about the product on the Black Stuff - Cheap Low Cost Carbon Fibre product page but basically what we've done is identify that there are lots of occasions where a more basic spec carbon fibre might be all that's needed and so we looked into what the lowest possible price such a cloth could be made for. What we came up with is a fibre that we can sell direct to customers at £10/sqm for a 10m roll or £9/sqm for a 100m roll. I think I can say with confidence this price has never been offered for this quantity, in the UK or across Europe.

The reason for the post is not really to promote the material, it's flying off the shelves and our first batch will be gone soon without my help but what I did want to do is see if anyone had used it yet and had any feedback on it or if anyone had any questions about it. It's easier to discuss these things in a thread than individually with customers Smile.

If you have used the fibre, let me know what you thought. To offer it at half the normal price clearly we have to compromise a bit and I'm interested to know what people think. Also, if you have any questions, I'm happy to answer them.

Best regards, Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
Replies
FLD
FLD
Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
I've recently used this for a few parts too.  The weave blemishes are over stated in the description as it really is rather good.  I've found one or two slight pulls but most of the blemishes seem to be sightly tight tows and the blemish is very minor.  It is just like regular 200g cloth.  I'm making car panels which will be painted so its ideal for me. 

I would also add a vote for a heavier material.  I buy 650g from ECF which is great.  Anything similar would be awesome.
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Thanks FLD, vote duly noted Smile. On the 650g front, we've always stocked and sold a very nice 650g 2/2 Twill 12k Carbon Fibre but I'm certainly now looking into getting a Black Stuff version of the cloth too.

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Matt (Staff) - 12 Years Ago
Brian2fast - 12 Years Ago
wozza - 12 Years Ago
Matt (Staff) - 12 Years Ago
Manu - 12 Years Ago
Matt (Staff) - 12 Years Ago
Superleggera - 12 Years Ago
Matt (Staff) - 12 Years Ago
Lawrence78 - 12 Years Ago
Matt (Staff) - 12 Years Ago
Brian2fast - 12 Years Ago
Matt (Staff) - 12 Years Ago
FLD - 12 Years Ago
Matt (Staff) - 12 Years Ago
ceebmoj - 12 Years Ago
Matt (Staff) - 12 Years Ago
FLD - 12 Years Ago
Matt (Staff) - 12 Years Ago
                 any further updates on delivery?
ceebmoj - 11 Years Ago
Matt (Staff) - 11 Years Ago
twissta - 11 Years Ago
twissta - 11 Years Ago
Matt (Staff) - 11 Years Ago
andygtt - 11 Years Ago
Matt (Staff) - 11 Years Ago
Bean Bandit - 11 Years Ago
Matt (Staff) - 11 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search