Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi Bean Bandit,

I'm not sure about a wider fabric. Again, I'm happy to consider your post as a vote for it but our future plans probably centre more around alternative weights than widths but I'll note that alternative widths have been enquired about too.

Best regards, Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi Andy,

The current Black Stuff Carbon Fibre 2/2 Twill 3k 200g uses a slightly lower strength fibre that our usual Carbon Fibre 2/2 Twill 3k 199g but it has a very similar tensile modulus.

Here's the comparison:

STANDARD (1ST GRADE)  -  4410MPa (tensile strength) - 235GPa (tensile modulus)
BLACK STUFF - 3450MPa (tensile strength) - 230GPa (tensile modulus)

Full details can be found on the SPECIFICATION tab on both products pages (for the black stuff and our standard fibre).

As you can see, the ultimate tensile strength (the amount of load at which the fibre would break) is lower although its tensile modulus (i.e. how stiff it is) is almost the same. This means that in terms of the stiffness of a panel, they would be very similar but the total load you could put on a panel before it would break would be lower with the BLACK STUFF. Its properties are still way ahead of alternative materials at a similar price.

--Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
Edited 11 Years Ago by Matt (Staff)
Bean Bandit
Bean Bandit
Supreme Being (116 reputation)Supreme Being (116 reputation)Supreme Being (116 reputation)Supreme Being (116 reputation)Supreme Being (116 reputation)Supreme Being (116 reputation)Supreme Being (116 reputation)Supreme Being (116 reputation)Supreme Being (116 reputation)
Group: Forum Members
Posts: 10, Visits: 136
Any chance for future black stuff in a slightly wider version (1.2m or more)?
andygtt
andygtt
Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)
Group: Forum Members
Posts: 157, Visits: 1.2K
Id be interested in a heavier grade... i tend to use pro carbon on the face and back with 650 if i need bulk, which would still be cheaper and easier.

other than looks does the 'blackstuff' have any structural drawbacks?
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
The 200g 2/2 Twill Black Stuff has just been delivered this morning. We're seriously considering what we could do (price wise) on heavier grades of the same material. Anyone who wants to snap up some bargain 200g 2/2 twill carbon will find it available to buy online here: https://www.easycomposites.co.uk/200g-black-stuff-22-twill-3k-carbon-fibre-cloth and then if we do something in the future on some heavier fabrics then I'll be sure to post an announcement.

All the best, Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
twissta
twissta
Supreme Being (381 reputation)Supreme Being (381 reputation)Supreme Being (381 reputation)Supreme Being (381 reputation)Supreme Being (381 reputation)Supreme Being (381 reputation)Supreme Being (381 reputation)Supreme Being (381 reputation)Supreme Being (381 reputation)
Group: Forum Members
Posts: 27, Visits: 341
I haven't since I really been posting on the site since I signed up when you first started. I have been practicing with and ready to move forward with my business. soon I will post some project pic's to get some feedback from the Talk Composite Family....!
twissta
twissta
Supreme Being (381 reputation)Supreme Being (381 reputation)Supreme Being (381 reputation)Supreme Being (381 reputation)Supreme Being (381 reputation)Supreme Being (381 reputation)Supreme Being (381 reputation)Supreme Being (381 reputation)Supreme Being (381 reputation)
Group: Forum Members
Posts: 27, Visits: 341
Hello Matt save some for me...LOL I have been waiting along time to get to this point and ready to get some of this Black Stuff to. Looking forward to the other weights too!
i
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Yes, we do. Material will be with us on or around the 16th of January (so this Friday). Lots of demand again by the looks of it but we have good stocks, initially anyway.

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
ceebmoj
ceebmoj
Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)
Group: Forum Members
Posts: 5, Visits: 29
any further updates on delivery?
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Thanks for the feedback FLD. Actually, we have trialled that packing method for all our fabrics and feedback (and our own opinion) was split between though that favour the brown paper and those that favour the bubblewrap. Generally, I'm on the bubblewrap side which is why that's what we normally use but it is interesting to hear your feedback, and that of others, which of course informs our opinions and decision on things such as this.

--Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search