Hello!

I have a question about  sandwich core technique.
That is...

For example,
If I use  two set of  5mm nomex honeycomb core(10mm thick in total) to  make a sandwich panel,
is it  as strong as  a single 10 mm nomex honecomb core panel?
the  double 5mm sandwich has reasonable strength?
or the double 5mm sandwich is easy to break?


actually,
I want to build a curved sandwich panel.
I tried a 10mm thick  nomex honeycomb core at first,
but the 10mm thick core was too strong to bend.

 I wonder that if I use  a 5mm core,then laminate,bend  and add one more 5mm honeycomb core.
I mean,,  the sandwich is   CFRP>honeycomb core(5mm)>CFRP>honeycomb core(5mm)>CFRP.
If this idea is O.K. I will be able to build thick and strong curved sandwich panels.


Any advice,
I would be happy.

Thanks,







 
Replies
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
As said, just pay careful attention to all your frame triangulation.  It is key to load distribution and keeping it light.  It would be real easy to make an over engineered wheelchair, but it would be over heavy too. The beauty of an already light and stiff material like carbon, is that even with over engineering, a slightly heavy carbon part is still lighter by a long way than a similar metal part and thus can still meet the persons needs, however when pushing the limits of svelte design you need to be a bit more precise and plan it carefully.

Do that and im sure you will create a awesome wheelchair.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
hietaka
hietaka
Supreme Being (118 reputation)Supreme Being (118 reputation)Supreme Being (118 reputation)Supreme Being (118 reputation)Supreme Being (118 reputation)Supreme Being (118 reputation)Supreme Being (118 reputation)Supreme Being (118 reputation)Supreme Being (118 reputation)
Group: Forum Members
Posts: 14, Visits: 169
> Warren san

Thanks!

I am re-designing CFRP wheelchair now.
maybe I will report it after proto-type is built.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
hietaka - 11 Years Ago
Warren (Staff) - 11 Years Ago
hietaka - 11 Years Ago
brainfart - 11 Years Ago
brainfart - 11 Years Ago
hietaka - 11 Years Ago
Warren (Staff) - 11 Years Ago
f1rob - 11 Years Ago
hietaka - 11 Years Ago
f1rob - 11 Years Ago
brainfart - 11 Years Ago
ChrisR - 11 Years Ago
Warren (Staff) - 11 Years Ago
hietaka - 11 Years Ago
hietaka - 11 Years Ago
Warren (Staff) - 11 Years Ago
hietaka - 11 Years Ago
f1rob - 11 Years Ago
hietaka - 11 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search