I have been working with carbon fiber since this year so I'm still a rookie I would say. I doing some CF myself and I'm wondering if I could use pre preg to do laminations of the nterior trim ?
Reply
TomRiddel
TomRiddel
Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)
Group: Forum Members
Posts: 3, Visits: 15
So manufacturing the part from pre preg would be the best idea ?