Stand Up Paddleboard infusion


Author
Message
andrew.spencer.2
andrew.spencer.2
Supreme Being (79 reputation)Supreme Being (79 reputation)Supreme Being (79 reputation)Supreme Being (79 reputation)Supreme Being (79 reputation)Supreme Being (79 reputation)Supreme Being (79 reputation)Supreme Being (79 reputation)Supreme Being (79 reputation)
Group: Forum Members
Posts: 5, Visits: 26
I was just having a gander at your charming resin infusion starter kit, and was wondering if it would fit my needs. I've only ever done wet hand layups in the past, so jumping straight into resin infusion vacuum bagging is a pretty big step for me. 

I watched the very helpful video tutorial on infusion which answered a lot of questions, but it's a little different from what I want to do, which is this:
Coat a 3.5m Stand Up Paddleboard (SUP, think really big surfboard) in carbon fibre. It's a hollow wooden affair, entirely sealed in sanding sealer as to be non-porous. 

Firstly, is it even possible to coat an object on all sides with a vacuum infusion? Should I try to do the top and bottom separately, or can I do it all in one go? What sort of resin should I use? How would I place the infusion feed spiral? 
Sorry for the barrage of questions, if anybody has answers, I would really appreciate some guidance.

Reply
Dravis
Dravis
Supreme Being (7.2K reputation)Supreme Being (7.2K reputation)Supreme Being (7.2K reputation)Supreme Being (7.2K reputation)Supreme Being (7.2K reputation)Supreme Being (7.2K reputation)Supreme Being (7.2K reputation)Supreme Being (7.2K reputation)Supreme Being (7.2K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
I would definitely go for Epoxy resins, for this sort of job...  (not just because I hate the stink of polyester)    As an afterthought, I would maybe add some fumed silica filler to the "base coat" if you make it yourself. That will stop it being quite so "runny" and make it easier to "paint on"  I would probably use a roller for something like this.

Epoxy will be just fine, even if exposed to sunlight/UV, if you get it clearcoated with a good 2-component Urethane  (I use 2-comp boat varnish, since I have access to it cheaply, and have my own spray-guns.)

BTW... I got "Sapere Aude" from a very good book called "Reckoning with Risk" by Gerd Gigerenzer... (Penguin books) Well worth a read, I assure you!! and also the inspiration for the second line in my signature  Smile

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
Edited 12 Years Ago by Dravis
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
andrew.spencer.2 - 12 Years Ago
ChrisR - 12 Years Ago
andrew.spencer.2 - 12 Years Ago
ChrisR - 12 Years Ago
Warren (Staff) - 12 Years Ago
andrew.spencer.2 - 12 Years Ago
ChrisR - 12 Years Ago
andrew.spencer.2 - 12 Years Ago
brainfart - 12 Years Ago
Dravis - 12 Years Ago
andrew.spencer.2 - 12 Years Ago
Warren (Staff) - 12 Years Ago
Dravis - 12 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search