I do think you will struggle trying to pull a full vacuum on that. Even wetlay vacuum bagging would likely cause the sagging issue between ribs.
You would need to do a wet lay up and just be very careful with your resin usage and consolidation. As said, peel ply can help soak up some excess resin.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|