Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - Product Specific Pages
»
Resin Infusion Starter Kit
»
Stand Up Paddleboard infusion
Stand Up Paddleboard infusion
Post Reply
Like
10
Prev
1
2
Jump To Page
Stand Up Paddleboard infusion
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
andrew.spencer.2
andrew.spencer.2
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 5,
Visits: 26
Oh, I see. I definitely wouldn't want to fill the board with resin. Although, with the sanding sealer liberally applied, I'm fairly certain it's airtight. I've had it in the water already, and it didn't absorb anything anyway. As far as deforming goes, I've attached a picture of what it looks like on the inside (has a plywood skin on the deck now). I can stand on it if that's any indication.
I've never pulled a mould off of anything before, your suggestion sounds awfully complicated to my feeble mind. If you'd really recommend steering clear infusion, I suppose I can always go back to hand layup.
Attachments
SAM_0143.jpg
(
1K views,
105.00 KB
)
Reply
Like
11
ChrisR
ChrisR
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 363,
Visits: 3K
Yes you could do both top and bottom at the same time but you mention it's hollow wood so infusing may not be the way to go (one little crack in the finish and it will suck all the resin into the hole and that's if you can pull full vacuum on it and prevent the core from deforming).
If you were wanting to infuse then I would make a 2 or 3 part mould off the core, infuse the top and bottom layers seperately, bond together after infusion and add a foaming epoxy or PU to make the core
Reply
Like
10
andrew.spencer.2
andrew.spencer.2
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 5,
Visits: 26
I was just having a gander at your charming resin infusion starter kit, and was wondering if it would fit my needs. I've only ever done wet hand layups in the past, so jumping straight into resin infusion vacuum bagging is a pretty big step for me.
I watched the very helpful video tutorial on infusion which answered a lot of questions, but it's a little different from what I want to do, which is this:
Coat a 3.5m Stand Up Paddleboard (SUP, think really big surfboard) in carbon fibre. It's a hollow wooden affair, entirely sealed in sanding sealer as to be non-porous.
Firstly, is it even possible to coat an object on all sides with a vacuum infusion? Should I try to do the top and bottom separately, or can I do it all in one go? What sort of resin should I use? How would I place the infusion feed spiral?
Sorry for the barrage of questions, if anybody has answers, I would really appreciate some guidance.
Cheers!
Andrew
Tags
carbon fiber
infusion
SUP
Surfboard
Reply
Like
10
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
10
Prev
1
2
Jump To Page
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search