So my brother and i decided to do our first infusion today and have a couple of questions. We wanted to do a small sample to get the idea of how to do it and didnt have the best success. We layered 2 sheets 0f .017 and 2 sheets of .010 CF at 8x10". We had plenty of resin but the infusion rate was really slow toward the end and eventually did not cover this small 8x10" piece. So i am trying to figure out what we did wrong. As you can see in the picture we had peel ply on top of CF then infusion mesh on ends with spiral tubing at inlet. Ran the pump for approximately 35 min before finally shutting off. We were using fiberglast system 2000 with 20 min epoxy hardener. Thoughts?
Reply
bewbzout
bewbzout
Supreme Being (96 reputation)Supreme Being (96 reputation)Supreme Being (96 reputation)Supreme Being (96 reputation)Supreme Being (96 reputation)Supreme Being (96 reputation)Supreme Being (96 reputation)Supreme Being (96 reputation)Supreme Being (96 reputation)
Group: Forum Members
Posts: 16, Visits: 46
Thank you for the replies. I am thinking our biggest problem was not using the infusion mesh across the whole part. My question though is without the peel ply how do you keep the part from sticking to the CF? Do you lay a full layer of peel ply then a full layer of infusion mesh? 

Oh I'm not sure about the resin but it is sold for doing this stuff. We chose the 20 min hardener because we figured this was a really small part and it should have covered faster. Are we wrong on thinking it will cover 8"x10" in 20 min? 

Thank you so much for the help
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
bewbzout - 11 Years Ago
bewbzout - 11 Years Ago
fgayford - 11 Years Ago
matthieutje65 - 11 Years Ago
brainfart - 11 Years Ago
brainfart - 11 Years Ago
bewbzout - 11 Years Ago
Hanaldo - 11 Years Ago
bewbzout - 11 Years Ago
ChrisR - 11 Years Ago
Hanaldo - 11 Years Ago
ChrisR - 11 Years Ago
ajb100 - 11 Years Ago
bewbzout - 11 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search