KingsleyHill
KingsleyHill
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 6,
Visits: 20
What is the accepted method of obtaining a nice edge on a kevlar part? All the methods I have tried (basically all the usual fiberglass and carbon fiber cutting and finishing techniques) result in a furry edge. I have tried tacking down the fur with resin but that results in hard Aramid/Kevlar hairs sticking up from the edge perfect for sticking into soft body parts. Suggestions?
Tags
Aramid
Cutting
Edges
Finishing
Kevlar
Reply
Like
10
Reply
r0bsk1
r0bsk1
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 38,
Visits: 307
Use diamond coated files
Reply
Like
10
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Cutting and Finishing Edges of Kevlar (Aramid) Part
KingsleyHill
-
12 Years Ago
Best way is to leave the kevlar away from the edge of the part so you don't have to cut it at all....
Hanaldo
-
12 Years Ago
I use 240 grit sand paper which seems to get the worst of the fluff off. For diolen, I use a blow...
ajb100
-
12 Years Ago
If you have to keep the Kevlar to the edge you can rub the edge down with 800/1000/1200 wet and dry...
f1rob
-
12 Years Ago
Wet sand it with 220 , all the fuzz will be gone
George Sychrovsky
-
12 Years Ago
Use diamond coated files
r0bsk1
-
12 Years Ago
Post Reply
Like
10
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search