What is the accepted method of obtaining a nice edge on a kevlar part?  All the methods I have tried (basically all the usual fiberglass and carbon fiber cutting and finishing techniques) result in a furry edge.  I have tried tacking down the fur with resin but that results in hard Aramid/Kevlar hairs sticking up from the edge perfect for sticking into soft body parts.  Suggestions?  
Reply
f1rob
f1rob
Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)
Group: Forum Members
Posts: 237, Visits: 4.8K
If you have to keep the Kevlar to the edge you can rub the edge down with 800/1000/1200 wet and dry and get a fairly smooth edge

Also sandwich the outside edge of the part in a carbon edge makes it easy to trim