How many layers of Biotex jute fibre plain weave 290 g are to be used for making of epoxy matrix composite sheets of 3 mm thickness by compression moulding process?
Reply
tack talk
tack talk
Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)
Group: Forum Members
Posts: 9, Visits: 215
I would use 8 layers assuming the following

Biotex Flax density = 1.46g/cm3
Epoxy resin density = 1.20g/cm3
Laminate has 43% rw