rbpatil
rbpatil
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 2,
Visits: 8
How many layers of Biotex jute fibre plain weave 290 g are to be used for making of epoxy matrix composite sheets of 3 mm thickness by compression moulding process?
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Layers of jute composites for 3 mm thick sheet.
rbpatil
-
11 Years Ago
I would use 8 layers assuming the following Biotex Flax density = 1.46g/cm3 Epoxy resin density =...
tack talk
-
11 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search