Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
GC50 Gelcoat question
GC50 Gelcoat question
Post Reply
Like
3
GC50 Gelcoat question
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
nickvancamp1
nickvancamp1
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 10,
Visits: 104
hey guys, i'm quite new into this and i had a question about the GC50 gelcoat.
I've read that the gelcoat actually isn't easy to brush apply on the mold, neither with a roller.
however, on the website they say it is possible.
Is it possible to give it 1 layer gelcoat, even if it has the 'fisheye' effect, let this layer cure, and then add a 2nd one to fill the rest of the inpurity's
(fisheye or other little dots).
would it be a good idea to sand the layer once its cured, so the carbon or kevlar wave can't be disturbed by an uneven coat?
sorry if it's a stupid question, but i dont know weither i'd buy the spraygun or try it with a brush first
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
GC50 Gelcoat question
nickvancamp1
-
11 Years Ago
Hi, I use GC50 a lot and for me it has to be spray applied. You may get away with roller application...
wozza
-
11 Years Ago
also if you must brush apply, only do it for wetlay parts. The brush marks when resin infused...
Warren (Staff)
-
11 Years Ago
then i suppose spraying will be the only way. i have a undercan spraygun wich is actually designed...
nickvancamp1
-
11 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search