By nickvancamp1
-
2/21/2014 9:07:38 AM
hey guys, i'm quite new into this and i had a question about the GC50 gelcoat.
I've read that the gelcoat actually isn't easy to brush apply on the mold, neither with a roller.
however, on the website they say it is possible.
Is it possible to give it 1 layer gelcoat, even if it has the 'fisheye' effect, let this layer cure, and then add a 2nd one to fill the rest of the inpurity's
(fisheye or other little dots).
would it be a good idea to sand the layer once its cured, so the carbon or kevlar wave can't be disturbed by an uneven coat?
sorry if it's a stupid question, but i dont know weither i'd buy the spraygun or try it with a brush first
By nickvancamp1
-
2/21/2014 9:44:05 AM
then i suppose spraying will be the only way.
i have a undercan spraygun wich is actually designed for underbody sealant and such, could this work or is the gellcoat spraygun the only way to go?