Brian2fast
|
|
|
Group: Forum Members
Posts: 79,
Visits: 1.3K
|
Hi All Xmas has arrived early up here in Scotland. Opened up my first big infusion of 2014/15 carbon season tonight. First time I used MTI hose and first time I attempted a V joint. Took a mould off my existing GRP and perspex aeroscreen. After the mould was made I sanded out the groove that was left in the mould where the GRP/perspex join was. Used Pro weave for the outer layer and cut the join with scissors then butted them up. then 3 layers of black stuff. Carried out 90% of the infusion with the resin feed at the same level as the mould then near the end dropped the resin cup down 1 meter and slightly before the resin hit the last of the MTI hose I clamped the resin feed off. No pin holes. Woohoo  |
|
|
|
|
Whitebits
|
|
|
Group: Forum Members
Posts: 9,
Visits: 31
|
This thread is truly inspirational
I''m building a race car! I believe that if life gives you lemons, you should make lemonade..and try to find somebody whose life''s given them vodka and have a party - Ron White Racing is life. Anything before or after is just waiting - Steve McQueen
|
|
|
|
|
Dravis
|
|
|
Group: Forum Members
Posts: 592,
Visits: 1.9K
|
I would not call myself an "expert" at infusion ... I probably only really have limited experience.. But:
Polyester resin is just pure trouble, even when trying to vac-bag it ... tried that .. did NOT like it...
I'v never used VinylEster, so no experience there..
I've tried at least four different resin systems for infusion, only one ( EC IN2) worked perfectly, given a perfectly sealed bag, no degassing, the resin degasses perfectly during the infusion, as far as I can see in my smallish projects.
I've infused West systems 105, and it works too, but has very slow infusion rates, again, it seems to degas fine during infusion. (completely Pin-hole free parts are rare with this resin)
EC EL2 seems almost identical to West 105 when infusing it. (Again almost always a small number of pinholes, my theory is that the higher viscosity resin traps more gas in the fabric.)
EC High temp will infuse, but it is near impossible to get pin-hole free parts. It helps to heat the resin to maybe 30 - 40 deg, but infusion then has to go quickly and without problems, or you may run into trouble with the resin either exotherming in the pot or gelling at the last part of infusion. Consequently I usually degas, wet-lay and Vac-bag, going rather resin rich.
"Sapere Aude"... Dare to KNOW!
The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...
103% of all people do not understand statistics...
Do not adjust our mind, theres a fault in reality :-)
|
|
|
|
|
brainfart
|
|
|
Group: Forum Members
Posts: 198,
Visits: 1.4K
|
> Unfortunately many forums have "armchair experts" who read a question, go off and google it and then copy and > paste answers from other sources. Not based on experience.
Nice.
> I certainly don't use statements like "Degas. Do It."
Taken out of context. You forgot to mention the lines before that statement. Degas, if there is visible frothing of the resin during the infusion.
|
|
|
|
|
wozza
|
|
|
Group: Forum Members
Posts: 688,
Visits: 5.4K
|
If you read any of my replies to people's questions they are all based around "what works/doesn't work for me" and never this is the only way to do things, all based on experience. I certainly don't use statements like "Degas. Do It." Unfortunately many forums have "armchair experts" who read a question, go off and google it and then copy and paste answers from other sources. Not based on experience. Warren
Carbon Copies Ltd
|
|
|
|
|
brainfart
|
|
|
Group: Forum Members
Posts: 198,
Visits: 1.4K
|
Let me quote this again:
> > When I have a line clamp not full open it seems to create bubbles,
This to me sounds like there are visible bubbling going on when the resin starts to infuse the part. So there is clearly some sort of outgassing taking place. (or did I totally misunderstand this sentence?)
If infusing parts works for you without degassing, fine, then do it without. Not using degassed resin is another source for error for the inexperienced. Just look how many posts and questions there are about infusing with (in my opinion usually unsuitable) VE and polyester resins. And epoxy resins of unknown origin, with god knows what volatile ingredients. Blanket statements like "degassing unnecessary" might be true sometimes but certainly not all of the time.
> The more processes you add into the mix the more chance there is of things going wrong, and trust me people get degassing wrong.
The main problem I see here is people not really understanding what is going on, and trying to get ahead of themselves. Infusion isn't exactly a simple process for beginners, people need to learn how to do a proper wet layup without vacuum bagging etc. before progressing to more advanced procedures.
And degassing is dead simple if you do it right. Like NOT trying to degas an enormously thick layer of resin in a narrow, high container. The thicker the layer to be degassed, the harder the process is because the vacuum at the bottom of the resin container is much worse than that at the top of the resin. Simple basic physics.
|
|
|
|
|
Hanaldo
|
|
|
Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
|
|
|
|
|
wozza
|
|
|
Group: Forum Members
Posts: 688,
Visits: 5.4K
|
|
|
|
|
|
Hanaldo
|
|
|
Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
MTI Hose is great Brian. Not always necessary, but because it makes it possible to develop a completely closed system, it can save some parts if something goes wrong.
|
|
|
|
|
wozza
|
|
|
Group: Forum Members
Posts: 688,
Visits: 5.4K
|
Shell should be going to the paint shop this week for top coat. Then we can start working out split lines and fitting flanges.  Warren
Carbon Copies Ltd
|
|
|
|