Group: Forum Members
Posts: 468,
Visits: 2.7K
|
Good lord! That's some ambitious project. WRT 'best fibre type' I would say unidirectional would be the best but you would first need to calculate the loads on the subframe and lay up in the right directions. From what I've seen of supercars most use carbon for the tub but then revert to metals for subframes / cross members etc. The reason being that they are far more durable than composites. I'm not sure how composites fatigue so you may find you're having to replace your cross member rather frequently. Consider the elise. This uses an alloy tub with a steel rear subframe. An alloy subframe and composite subframe were investigated but were unsuitable for this reason.
|