Group: Forum Members
Posts: 468,
Visits: 2.7K
|
Nice find!
I reuse gum tape. On a flanged mould, if yourecareful, you can get the bag to leave the tape on the mould. I usually hand lay and bag so if I want a foam core I lay one skin, pull off the bag and lay in the core, bag that, pull off the bag and lay in the second skin. I get all three out of one lot of tape. The only extra bits I have to add are for the pleats.
I must admit that this only seems to work with the EC tape, I've tried others and found the tape a bit firmer so it doesn't seem to cope with re-use so well. The EC stuff really is top notch.
|