Joe
Joe
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 310,
Visits: 1.5K
Wow, Steve, thats quite a great project. The telescope itself looks great.
And, also being a machinist (not on cnc, sadly), I cant stop staring at your polished mold. Something I could hang on my wall above my fireplace just because its way more beautiful than a Picasso to me
 
 
    A $1000 electronic device will always protect a 10 cents fuse
Reply
Like
6
steveastroUK
steveastroUK
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 21,
Visits: 78
Thanks Joe. It is a pretty thing. The learning curve to make it was interesting too. The final job took about three hours to do 90% of the hogging - and 18 hours on the finish cut !
Here's a better view of the whole thing.
Steve
Edited
14 Years Ago by
steveastroUK
Reply
Like
7
Joe
Joe
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 310,
Visits: 1.5K
Thanks for the additional picture, this one really gives the telescope justice! Congrats for this sweet looking piece of art.
 
 
    A $1000 electronic device will always protect a 10 cents fuse
Reply
Like
7
brummelisa
brummelisa
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 20,
Visits: 144
Hi,
I have finally finished my frame.
I copied a Cervelo P5 (I took a photo and used it as a measurement).
It took three months (don't know exact how many hours I put into it).
Anyway, here are the photos of it...
The word LELLOU and BOBBO is my nickname for my two children.
Not much room between the wheel and the frame
The image above is of my two kids (the image is under the clear-coat and it's a bit fuzzy here, but the image is this one:
http://lellou.com/index.php?showimage=40&category=0
And the wheel is tight here too...
The part above (right where the wheel is fastened) has 40 layers of CF. It's 8 mm thick and it was a pain in the a... to saw through it.
Tags
frame
Reply
Like
6
Wabba
Wabba
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 21,
Visits: 64
Brummelisa,
That bike is impressive, and I don't even ride bikes
Big thumbs up.
Reply
Like
6
Pertabolis
Pertabolis
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 17,
Visits: 193
Hi
Brummelisa
That really impressive !
BTW how would such a frame cost in raw mat (fiber and epoxy) ? I guess this is nothing compare to the time you took to build this though.
Pierrre
Reply
Like
6
brummelisa
brummelisa
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 20,
Visits: 144
I bought six meters of CF and two liters of resin.
I think I ended up using almost 5 meters of CF and I don't know exactly how much resin, but the two liters was used up, but naturally everything isn't on the bike, but a lot is in the dustbin
The frame's weight is around 1700 and that is too me a bit much, but ok for the first frame
Reply
Like
4
kylle
kylle
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 34,
Visits: 101
Nice Bike !!!!
My project room is also finished some pic's:
http://www.carbonwork.pt/DSC05373.JPG
http://www.carbonwork.pt/DSC05375.JPG
http://www.carbonwork.pt/DSC05385.JPG
http://www.carbonwork.pt/DSC05381.JPG
Reply
Like
12
steveastroUK
steveastroUK
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 21,
Visits: 78
Also available in black......
Final production case, thermal compression moulded.
Shiny aluminium bit is for calibration only !
Very chuffed. First orders coming in a couple of weeks.
Reply
Like
6
bruce77
bruce77
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Awaiting Activation
Posts: 2,
Visits: 12
Hi to everyone, some shots of my last work. I hope you like
Attachments
1a.jpg
(
1,000 views,
511.00 KB
)
1b.jpg
(
898 views,
507.00 KB
)
1d.jpg
(
845 views,
603.00 KB
)
1e.jpg
(
826 views,
725.00 KB
)
1g.jpg
(
826 views,
847.00 KB
)
1h.jpg
(
804 views,
622.00 KB
)
1o.jpg
(
827 views,
746.00 KB
)
Tags
helmet
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
19
Prev
1
3
4
5
6
7
20
Next
Jump To Page
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search