Coating a 3d printed part
Coating a 3d printed part
Post Reply
Like
2
Coating a 3d printed part
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
GeorgeK
GeorgeK
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 1,
Visits: 6
Hi,
I have recently had some prototype parts 3d printed for testing. Unfortunately the geometry did not allow for coating/polishing. I was thinking, maybe I could dip my models in a relatively low viscosity resin (or ideally rubber) in order to allow the resin to enter the pores of my part and then allow to polymerize thus creating a better surface. Do you have any ideas on whether this is possible or not? Could I perhaps use some sort of thinner to achieve a lower viscosity without slowing the polymerization process down too much? Spraying the resin on the part is also an option, but again it would need to have a low viscosity.
Thanks in advance,
George
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Coating a 3d printed part
GeorgeK
-
12 Years Ago
You could try our IN2Epoxy Infusion Resin as its the thinnest resin we have. It...
Warren (Staff)
-
12 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search