You could try our IN2Epoxy Infusion Resin as its the thinnest resin we have.

It depends on the material as well.  Perhaps test a sample piece with wax as waxes can fill pores.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GeorgeK
GeorgeK
Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)
Group: Forum Members
Posts: 1, Visits: 6
Hi,

I have recently had some prototype parts 3d printed for testing. Unfortunately the geometry did not allow for coating/polishing. I was thinking, maybe I could dip my models in a relatively low viscosity resin (or ideally rubber) in order to allow the resin to enter the pores of my part and then allow to polymerize thus creating a better surface. Do you have any ideas on whether this is possible or not? Could I perhaps use some sort of thinner to achieve a lower viscosity without slowing the polymerization process down too much? Spraying the resin on the part is also an option, but again it would need to have a low viscosity.

Thanks in advance,

George