I use molds milled from solid surface material (corean). It is usually used for high quality kitchen worktops and if you are lucky you can find kitchen fabricators who will let you take their spare offcuts for a really good price.

I've also used ebalta pw920 which is designed for the job, but it  is not cheap but cuts like butter on the cnc.

Aluminium molds look amazing, but are expensive and have a very different rate of expansion so can be tricky when molding larger items. My CNC is not really up to the job of milling aluminium.
Matthieu Libeert
Matthieu Libeert
Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
Hi,

So I have a small question,
Did anyone on here ever made a CNC-milled design out of a certain material like Aluminium, Steel, Epoxy-foam... that is prepreg-ready (110-120°C).
What are your experiences, what materials used, How were the results, what was the finish on the part....

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




Tags
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search