Most plastic compatable paints are fine.  Otherwise you can use a plastic primer.  You will need to key the surface prior to painting as will all other materials.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Perfectphase
Perfectphase
Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)
Group: Awaiting Activation
Posts: 2, Visits: 28
Hi all,  is it possible to paint the Fast Cast Polyurethane Casting Resin with standard cellulose/acrylic spray cans?

Cheers,

Stephen.
Edited 12 Years Ago by Perfectphase
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search