Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - General Technical Support
»
Painting Fast Cast Polyurethane Casting Resin
Painting Fast Cast Polyurethane Casting Resin
Post Reply
Like
2
Painting Fast Cast Polyurethane Casting Resin
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Perfectphase
Perfectphase
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Awaiting Activation
Posts: 2,
Visits: 28
Hi all, is it possible to paint the
Fast Cast Polyurethane Casting Resin with standard cellulose/acrylic spray cans?
Cheers,
Stephen.
Edited
12 Years Ago by
Perfectphase
Reply
Like
2
Warren (Staff)
Warren (Staff)
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
Most plastic compatable paints are fine. Otherwise you can use a plastic primer. You will need to key the surface prior to painting as will all other materials.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search