By Perfectphase - 6/30/2013 11:59:59 PM

Hi all,  is it possible to paint the Fast Cast Polyurethane Casting Resin with standard cellulose/acrylic spray cans?

Cheers,

Stephen.
By Warren (Staff) - 7/1/2013 10:47:50 AM

Most plastic compatable paints are fine.  Otherwise you can use a plastic primer.  You will need to key the surface prior to painting as will all other materials.