Hi everybody!

I have ageneral question. The wrinkles formed in de vacuum bag of complex shapes will be tranferred to the rear surface of the part? If so, how can I avoid it? Thanks!      
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
you could use a peelply... peelply will remove all the excess (wrinkles) laying on top... and leave a nice finish... at least I think it looks cool BigGrin whats the technique you'r using? Vacuum baggin, infusion, prepreg?

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




alebassa
alebassa
Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)
Group: Forum Members
Posts: 48, Visits: 171
If you put down the peel ply smooth (maybe with some cuts in complex shapes) then you can avoid the wrinkles...


Alessandro
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search