Talk Composites - The Forum for Advanced Composites

wrinkles in vacuum bagging?

http://www.talkcomposites.com/Topic6852.aspx

By chemie29 - 6/30/2013 9:53:03 AM

Hi everybody!

I have ageneral question. The wrinkles formed in de vacuum bag of complex shapes will be tranferred to the rear surface of the part? If so, how can I avoid it? Thanks!      
By alebassa - 7/27/2013 9:49:16 AM

If you put down the peel ply smooth (maybe with some cuts in complex shapes) then you can avoid the wrinkles...