TomDesign
TomDesign
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 454, Visits: 2.5K
please numbers of resin that way i know which is bad and which is uv protected like you say?
morepower
morepower
Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)
Group: Forum Members
Posts: 242, Visits: 1.2K
carboncactus (25/06/2013)
morepower (25/06/2013)
 PRF will do 5m but I may need a couple of meters too so if we get a 10m roll and split it. It might be perfect..... I have to check how much VTF I have....


Which resin system and Diolen weight would it be? I quoted for 25m of 265g on RF464 (low temp)
 That is fine.. It is the stuff I used last time with the VTF suface and the SHD backing material and it was compatible with both..
morepower
morepower
Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)
Group: Forum Members
Posts: 242, Visits: 1.2K
TomDesign (25/06/2013)
PLEASE NUMBER OF RESIN OR SMTH AS MARINE RESIN NO ONE SELL HERE


Any Lloyds approved resin is fine and almost all polyester resin is UV stable. I use lloyds approved from a number of suppliers like Eastcoast Fibreglass or MBFG.
TomDesign
TomDesign
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 454, Visits: 2.5K
PLEASE NUMBER OF RESIN OR SMTH AS MARINE RESIN NO ONE SELL HERE
TomDesign
TomDesign
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 454, Visits: 2.5K
WARREN I NEED MANUFACTURER OR NUMBER OF RESIN SO I ASK PEOPLE HERE AS NO ONE SELL MARINE RESIN!
carboncactus
carboncactus
Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)
Group: Forum Members
Posts: 243, Visits: 1K
morepower (25/06/2013)
 PRF will do 5m but I may need a couple of meters too so if we get a 10m roll and split it. It might be perfect..... I have to check how much VTF I have....


Which resin system and Diolen weight would it be? I quoted for 25m of 265g on RF464 (low temp)

http://www.talkcomposites.com/Uploads/Images/db628ad5-e0e7-47b9-873a-3d84.png
Edited 13 Years Ago by carboncactus
wozza
wozza
Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Any Marine grade Polyester will give good U.V protection.Smile

Carbon Copies Ltd
TomDesign
TomDesign
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 454, Visits: 2.5K
STILL NO REPLY PLEASE LET ME KNOW WHICH POLYSTER RESIN YOU USE OR ANY LINK THAT NOT NEED CLEAR COAT ONLY POLISHING??
morepower
morepower
Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)
Group: Forum Members
Posts: 242, Visits: 1.2K
carboncactus (24/06/2013)
morepower (24/06/2013)
I use pre-preg Diolen ...


I need some prepreg Diolen sharpish. Just emailed PRF for a quote on a 25m roll, but only need about 5 metres. Let me know if you wanna do a group buy. I'm gonna have to get a roll of VTF as well soon.... Doze How are you doing for VTF?


Bear with me...lol... I have a little issue with a customer of our mutual friend.... he paid for a kit direct to ****s and then didnt want to pay more... Now he does.. so it is an on/off/on sale so as he didnt want the kit I sold it as it was taking up space... So it looks like I will need some more...Of both..... PRF will do 5m but I may need a couple of meters too so if we get a 10m roll and split it. It might be perfect..... I have to check how much VTF I have....
carboncactus
carboncactus
Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)
Group: Forum Members
Posts: 243, Visits: 1K
morepower (24/06/2013)
I use pre-preg Diolen ...


I need some prepreg Diolen sharpish. Just emailed PRF for a quote on a 25m roll, but only need about 5 metres. Let me know if you wanna do a group buy. I'm gonna have to get a roll of VTF as well soon.... Doze How are you doing for VTF?

http://www.talkcomposites.com/Uploads/Images/db628ad5-e0e7-47b9-873a-3d84.png